G-Tek® 3RX™

15针环保纱掌浸点珠丁腈发泡通用手套

31-5131R

4121

EN 388 2016 Results: 4121X
Abrasion: 4
Cut (Coupe Test): 1
Tear: 2
Puncture: 1
Cut (TDM-100 Test): X
Impact Protection:

EN 388 is a European Standard. Cut Level is determined by the number of cycles it takes a spinning circular blade, that is pulled across the material under a constant weight of 500 grams, to cut the fabric. As the number of cycles increase, so does the glove's ratings. Click here for more information about the EN 388 2016 standard.

ansi-abrasion-4
ANSI Abrasion Level: 4
Test Method: ASTM D3884-09

The ANSI/ISEA 105-2016 standard outlines test methods for abrasion and is scored from 0-6. The ASTM D3884-09 is used for uncoated gloves and the end point (failure) is the number of abrasion cycles when the first thread or yarn is broken. The larger numbers of cycles indicates greater abrasion resistance of the product and a higher ANSI Abrasion Level.

ANSI Puncture Level: 1
Test Method: ASTM F1342

The ANSI/ISEA 105-2016 blunt force puncture testing uses a probe to simulate a tear or burst hazard. The test measures the amount of force needed for a blunt probe to pierce through PPE material. Results are given in Newtons, which is converted into a 1-5 scale and spans from 10 newtons (Level 1) to 150+ newtons (Level 5) of puncture resistance.

Available Colors:

Black
  • SIZES: XS-XL
  • Packed: 120 Pair/Case
  • Country of Origin: China
Product Description

Product Description

适用于安全的干握和耐油

零件和材料的处理和组装

设备维护与维修

零件清洗

紧固和锚固

Features

  • 60% 回收塑料纱线 +10% 氨纶手套芯舒适灵活
  • 编织手腕有助于防止污垢和碎片进入手套
  • 丁腈发泡涂层涂层潮湿 / 油性情况抓握力良好
  • 掌部点珠增加抓握力
  • 耐接触温度高达 100° C
Standards Met

EN 388 2016 Results: 4121X

Abrasion: 4 Cut (Coupe Test): 1 Tear: 2 Puncture: 1 Cut (TDM-100 Test): X Impact Protection:

EN 388 is a European Standard. Cut Level is determined by the number of cycles it takes a spinning circular blade, that is pulled across the material under a constant weight of 500 grams, to cut the fabric. As the number of cycles increase, so does the glove's ratings. Click here for more information about the EN 388 2016 standard.

ANSI Abrasion Level: 4

ansi-abrasion-4

Test Method: ASTM D3884-09

The ANSI/ISEA 105-2016 standard outlines test methods for abrasion and is scored from 0-6. The ASTM D3884-09 is used for uncoated gloves and the end point (failure) is the number of abrasion cycles when the first thread or yarn is broken. The larger numbers of cycles indicates greater abrasion resistance of the product and a higher ANSI Abrasion Level.

ANSI Puncture Level: 1

Test Method: ASTM F1342

The ANSI/ISEA 105-2016 blunt force puncture testing uses a probe to simulate a tear or burst hazard. The test measures the amount of force needed for a blunt probe to pierce through PPE material. Results are given in Newtons, which is converted into a 1-5 scale and spans from 10 newtons (Level 1) to 150+ newtons (Level 5) of puncture resistance.